Research on the Durability Improvement Technology in the Negative Moment Regions of Steel-concrete Composite Continuous Beam
SUN Zonglei1, AI Zongliang2, ZHANG Yuhan2
1. China Railway Economic and Planning Research Institute, Beijing 100038, China; 2. China Railway Eryuan Engineering Group Co. Ltd, Chengdu, Sichuan 610031, China
Abstract:Research purposes: In order to further improve the structural durability, considering large dead load and live load of railway, taking 4×40 m railway steel-concrete composite continuous beam as an example, based on finite element analysis software Midas Civil, the feasibility and force behavior of uplift restricted-slip free studs of railway are studied. Research conclusions: (1) After the use of uplift restricted-slip free studs in the negative moment regions, the deflection of structure, beam-end rotation angle and natural frequency are little variable compared with the conventional shear studs, which has only little impact on the overall performance of steel beam. (2) It is recommended to use uplift restricted-slip free studs at the range of 0.15L (L is the beam span) at both sides of the middle fulcrum. (3) The transition regions on both sides are actually constraint-strengthening regions, and it's necessary to pay special attention to the studs setting in this area, ensuring that the first row of studs of transition regions meet the requirements of strength and fatigue performance. (4) The arrangement of studs on the narrow flange of I section is limited, and it has poor adaptability to the transitional strengthening area which shall be set for the uplift restricted-slip free studs. (5) The research results can provide references for the durability improvement in the negative moment regions of steel-concrete continuous beam bridge of passenger and freight railway.
孙宗磊, 艾宗良, 张誉瀚. 钢-混结合连续梁负弯矩区耐久性提升技术研究[J]. 铁道工程学报, 2022, 39(12): 54-59.
SUN Zonglei, AI Zongliang, ZHANG Yuhan. Research on the Durability Improvement Technology in the Negative Moment Regions of Steel-concrete Composite Continuous Beam. Journal of Railway Engineering Society, 2022, 39(12): 54-59.
田山坡. 钢混组合梁剪力连接件的计算方法研究[J]. 铁道工程学报,2014(8):56-61.Tian Shanpo. Research on the Calculation of Shear Connector of Steel Concrete Composite Beam[J]. Journal of Railway Engineering Society,2014(8):56-61.
[2]
中国公路学报编辑部. 中国桥梁工程学术研究综述·2021[J]. 中国公路学报,2021(2):1-97.Editorial Department of China Journal of Highway and Transport. Review on China’s Bridge Engineering Research: 2021[J].China Journal of Highway and Transport,2021(2):1-97.
[3]
戴晓春,王应良,游励晖,等. 跨大型铁路编组站钢-混组合梁斜拉桥体设计[J]. 高速铁路技术,2018(5):48-52.Dai Xiaochun,Wang Yingliang,You Lihui,etc. Overall Design of Steel-Concrete Composite Girder Cable-Stayed Bridge across Large Railway Marshalling Station[J]. High Speed Railway Technology,2018(5):48-52.
[4]
胡志坚,于善利,李刚. 预应力钢-混箱形组合连续梁负弯矩区开裂分析[J]. 桥梁建设,2020(4):66-71.Hu Zhijian,Yu Shanli,Li Gang. Analysis of Cracking in Hogging Moment Zone of Continuous Prestressed Steel-Concrete Box Composite Girder[J]. Bridge Construction,2020(4):66-71.
[5]
安景峰,刘礼威,郭赵元,等. 钢混组合钢板梁桥混凝土开裂影响因素及裂缝控制措施[J]. 南京工业大学学报:自然科学版,2020(3):389-398.An Jingfeng,Liu Liwei,Guo Zhaoyuan,etc. Factors Affecting Cracking and Crack Control Measures of Steel-concrete Composite Girder Bridge[J]. Journal of Nanjing Tech University:Natural Science Edition,2020(3):389-398.